Vyncolit FM 3000 Novolac Phenolic
Subcategory: Phenolic; Thermoset; Polymer
Material Notes: Self-lubricated cellulose reinforced phenolic molding compound modified for applications requiring reduced friction and low wear.Information provided by Vyncolit, a Sumitomo Bakelite Group
| Available Properties |
- Density
- Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell M
- Tensile Strength at Break
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- Dielectric Strength
- CTE, linear 20°C
- Deflection Temperature at 1.8 MPa (264 psi)
- Color
- Form
- Main Filler
- Molding Method
|
|
|
|