CP-Polymer-Technik Wellamid® 6000 GVZ 30 HWCP 30% Glass Fiber Z-Qualities Nylon 6, Heat Stabilized, Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Information provided by CP-Polymer-Technik GmbH & Co. KG
Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dielectric Loss Index
- Melting Point
- Melt Temperature
- Mold Temperature
- Back Pressure
- Holding Pressure
- Injection Speed
- Screw Speed
|
|
|
|
Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
|