CP-Polymer-Technik Wellamid® 6000 MX 400 CP Combination Nylon 6, Heat Stabilized, Dry
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Information provided by CP-Polymer-Technik GmbH & Co. KG
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dielectric Loss Index
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Back Pressure
- Holding Pressure
- Injection Speed
- Screw Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|