Westlake Polymers EF 601 LDPE
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: Heavy Duty Bags, Heavy Duty Shipping Sacks, Industrial Shrink Film, Heavy Duty C&A Sheeting
Material Notes: Applications- Heavy Duty Bags
- Heavy Duty Shipping Sacks
- Industrial Shrink Film
- Heavy Duty C&A Sheeting
Properties- Excellent Impact Strength
- Good Tear Strength
- Good Tensile Properties
- Good Heat Sealability
FDA: This material complies with FDA regulations in 21 CFR, section 177.1520, paragraph C, section 2.1, for use in articles that contact food. Kosher approved Processing: Extrusion melt temperatures of 375° to 410°F are recommended for Westlake Polymers EF 601 with blow-up ratios of 1.5:1 or higher. Information provided by Westlake Chemical Corporation
| Available Properties |
- Density
- Thickness
- Melt Index of Compound
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Coefficient of Friction
- Dart Drop
- Dart Drop Test
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Melt Temperature
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|