|   Westlake Polymers EF 607 Low Density Polyethylene  Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer Material Notes: Applications
 PropertiesHigh Drawdown Garment Films Laundry and Dry Cleaning Films 
 Excellent Drawdown Excellent Processability Good Heat Sealability Good Contact Clarity 
 FDA: This material complies with FDA regulations in 21 CFR, section 177.1520, paragraph C, section 2.1, for use in articles that contact food. Kosher approved  Processing: Extrusion melt temperatures of 300° to 330°F are recommended for Westlake Polymers EF 607 with blow-up ratios of 1.5:1 or higher. Information provided by Westlake Chemical Corporation 
| | 
    | Available Properties |  
    | DensityThicknessMelt Index of CompoundFilm Elongation at Break, MDFilm Elongation at Break, TDDart DropDart Drop TestFilm Tensile Strength at Break, MDFilm Tensile Strength at Break, TD1% Secant Modulus, MD1% Secant Modulus, TDMelt Temperature
 | 
 | 
 |  | | 
    | Property Data |  
    | 
    This page displays only the textof a material data sheet.
 
 To see MatWeb's complete data
 sheet for this material (including
 material property data, metal
 compositions, material suppliers,
 etc), please click the button below.
 |  
    |  | 
 | 
 | 
 |