Westlake Polymers EF 310 Low Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Material Notes: Applications- High Clarity Packaging Film
- Soft Goods Packaging
- Bakery Bags
- Bags for Textile Items
Properties- Excellent Optics
- Good Toughness
- Good Heat Sealability
- Good Processability
FDA: This material complies with FDA regulations in 21 CFR, section 177.1520, paragraph C, section 2.1, for use in articles that contact non-alcoholic food. Kosher approved Processing: Westlake Polymers EF 310 processes on conventional cast film extrusion equipment with recommended melt temperatures of 500° to 550°F. Information provided by Westlake Chemical Corporation
| Available Properties |
- Density
- Thickness
- Melt Index of Compound
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Dart Drop
- Dart Drop Test
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Haze
- Gloss
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|