Westlake Polymers EF 378 Low Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Material Notes: Applications- Diaper Liners
- General Purpose Clarity Applications
Properties - Good Haze and Gloss
- Good Processability
- Good Heat Sealability
- Good Strength
FDA: This material complies with FDA regulations in 21 CFR, section 177.1520, paragraph C, section 2.1, for use in articles that contact non-alcoholic food. Maximum film thickness is 0.0047 in. Kosher approved Processing: Extrusion melt temperatures of 500° to 550°F are recommended for Westlake Polymers EF 378 Information provided by Westlake Chemical Corporation
| Available Properties |
- Density
- Thickness
- Melt Index of Compound
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Dart Drop
- Dart Drop Test
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Haze
- Gloss
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|