Westlake Polymers EC 472 LDPE
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: Milk Cartons, Liquid Containers, Multiwall Bag Stock, Frozen Food Containers
Material Notes: Applications- Milk Cartons
- Liquid Containers
- Multiwall Bag Stock
- Frozen Food Containers
Properties - High Grease Resistance
- Good Drawdown
- Excellent Adhesion to Substrates
- Very Good Heat Sealability
- Very Good Moisture Barrier
FDA: This material complies with FDA regulations in 21 CFR, section 177.1520, paragraph C, section 2.1, for use in articles that contact food. Kosher approved Processing: The very good flow properties of Westlake Polymers EC 472 permit high-speed coatings at weights from 4 lbs. / 3,000 sq. ft. and up. Suggested melt temperatures range for extrusion coating EC 472 is 575° to 625°F. Information provided by Westlake Chemical Corporation
| Available Properties |
- Density
- Water Vapor Transmission
- Oxygen Transmission
- Nitrogen Transmission
- Carbon Dioxide Transmission
- Melt Index of Compound
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Vicat Softening Point
- Melt Temperature
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|