Westlake Polymers EC 477 Low Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Material Notes: Applications- Medium and Light Weight Coatings and Laminations
- Coated on Substrates to Provide Heat Sealability
- Hot Melt Laminating Adhesive
- General Purpose Coating
Properties - Excellent Adhesion
- Very Low Neck-in
- Excellent Heat Sealability
- Very Good Drawdown
- Good Moisture Barrier
FDA: This material complies with FDA regulations in 21 CFR, section 177.1520, paragraph C, section 2.1, for use in articles that contact food. Kosher approved Processing: Westlake Polymers EC 477 is one of the most easily processed polyethylene coatings. Excellent draw down and relatively low viscosity permits high line speeds at weights as low as 4 lbs. / 3,000 sq. ft. Low sensitivity to fluctuations in melt temperature allows Westlake Polymers EC 477 to be easily processed at melt temperatures of 575° to 625°F. For heavy coatings onto cellophane, 570°F is recommended. Neck-in is minimized, odor and smoke is reduced. Information provided by Westlake Chemical Corporation
| Available Properties |
- Density
- Water Vapor Transmission
- Oxygen Transmission
- Nitrogen Transmission
- Carbon Dioxide Transmission
- Melt Index of Compound
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Vicat Softening Point
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|