Westlake Polymers EF 464 Low Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Material Notes: Applications Properties - Good Toughness
- Good Processability
- Excellent Optical Properties
FDA: This material complies with FDA regulations in 21 CFR, section 177.1520, paragraph C, section 2.1, for use in articles that contact food. Kosher approved Processing: Extrusion melt temperatures of 250° to 280°F are recommended for Westlake Polymers EF 464 Information provided by Westlake Chemical Corporation
| Available Properties |
- Density
- Melt Index of Compound
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Stiffness
- 1% Secant Modulus
- Vicat Softening Point
- Melt Temperature
|
|
|
|