Westlake Polymers LF 2010 LLDPE
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Key Words: Bags and Sacks, Agricultural Films, Trash Bags and Liners, Coextruded Structures
Material Notes: Applications- Bags and Sacks
- Agricultural Films
- Trash Bags and Liners
- Coextruded Structures
Properties - Excellent Stiffness
- Excellent Resistance to Load Deformation
FDA: This material complies with FDA regulations in 21 CFR, section 177.1520, paragraph C, section 3.1a. Kosher approved Processing: Melt temperatures of 400° to 420°F are recommended for Westlake Polymers LF 2010 with blow-up ratios of 2:1 or higher. Information provided by Westlake Chemical Corporation
| Available Properties |
- Density
- Thickness
- Melt Index of Compound
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Dart Drop
- Dart Drop Test
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Haze
- Melt Temperature
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|