Westlake Plastics Absylux® FR Acrylonitrile-Butadiene-Styrene Flame Retardant

 

Subcategory: ABS Polymer; Thermoplastic; Polymer; ; ;

Material Notes:
Absylux ABS is a low cost engineering plastic that is easy to machine and fabricate. It is an ideal material for structural applications when impact resistance, strength, and stiffness are required. Absylux is widely used for machining preproduction prototypes since it has excellent dimensional stability and is easy to paint and glue. This is also available in flame retardant grade.

Information provided by Westlake Plastics.

Available Properties
  • Cost, 1 to 10 (Nylon = 2)
  • Density
  • Hardness, Rockwell R
  • Tensile Strength @ Yield
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Yield Strength
  • Compressive Strength
  • Compressive Modulus
  • Machinability (1-10; 1 = easiest)
  • Dimensional Stability (1-4; 4 = highest)
  • Izod Impact, Notched
  • Dielectric Strength
  • CTE, linear 68°F
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Flammability, UL94
  • Black
  • Natural (off white)
  • FDA
  • USDA
  • UV Resistance (1-4; 4 = highest)
  • Acetaldehyde Aq. (40%)
  • Acetic Acid Aq. (10%)
  • Acetone
  • Acrylonitrile
  • Aluminum Chloride Aq. (10%)
  • Aluminum Sulfate Aq. (10%)
  • Ammonia Aq. (10%)
  • Ammonia Gas
  • Ammonium Carbonate Aq. (10%)
  • Ammonium Chloride Aq. (10%)
  • Ammonium Chloride Aq. (37%)
  • Amyl Acetate
  • Amyl Alcohol
  • Aniline
  • Antimony Trichloride Aq. (10%)
  • Barium Chloride Aq. (10%)
  • Barium Sulfate Aq. (10%)
  • Barium Sulfide Aq. (10%)
  • Benzaldehyde
  • Benzene
  • Benzoic Acid Aq. (SAT)
  • Benzyl Alcohol
  • Bitumen
  • Bleaching Lye (10%)
  • Boric Acid Aq. (10%)
  • Bromine Aq. (30%)
  • Bromine Liq.
  • Butyl Phthalate
  • Butyric Acid (CONC)
  • Butyric Acid Aq. (20%)
  • Calcium Chloride Aq. (10%)
  • Calcium Hypochlorite
  • Camphor
  • Carbon Disulphide
  • Carbon Tetrachloride
  • Chlorine Aq. (10%)
  • Chlorine Gas (100%)
  • Chloroacetic Acid Aq. (10%)
  • Chlorobenzene
  • Chloroform
  • Chromic Acid Aq. (1%)
  • Citric Acid Aq. (10%)
  • Citric Acid Aq. (SAT)
  • Creosote
  • Cresols
  • Cresylic Acid
  • Cupric Sulfate Aq. (0.5%)
  • Cupric Sulfate Aq. (10%)
  • Cupric Sulfate Aq. (SAT)
  • Cyclohexanol
  • Cyclohexanone
  • Detergents, Organic
  • Dibutylphthalate
  • Dichlorodifluoro Methane
  • Dichloroethylene
  • Diethyleneglycol Aq. (90%)
  • Dimethyl Aniline
  • Dimethyl Formamide
  • Dioxane
  • Ethanol, Denatured (96%)
  • Ether, Diethyl
  • Ethyl Acetate
  • Ethyl Chloride
  • Ethylene Chloride
  • Ethylene Chlorohydrin
  • Ethylene Diamine
  • Ethylene Dichloride
  • Ethylene Glycol Aq. (96%)
  • Ferric Chloride Aq. (10%)
  • Ferric Chloride Aq. (5%)
  • Ferric Chloride Aq. (SAT)
  • Ferrous Chloride Aq. (10%)
  • Fluorine (Gas Wet)
  • Fluorosilicic Acid Aq.
  • Formaldehyde Aq. (10%)
  • Formic Acid Aq. (10%)
  • Formic Acid Aq. (3%)
  • Freon 12 (Arcton 12)
  • Fruit Juices (CONC)
  • Furfural
  • Gasoline
  • Glycerine
  • Heptane
  • Hexane
  • Hydrobromic Acid Aq. (10%)
  • Hydrochloric Acid Aq. (0.4%)
  • Hydrochloric Acid Aq. (10%)
  • Hydrochloric Acid Aq. (2%)
  • Hydrofluoric Acid Aq. (4%)
  • Hydrogen Peroxide Aq. (0.5%)
  • Hydrogen Peroxide Aq. (1%)
  • Hydrogen Peroxide Aq. (3%)
  • Iodine (3%)
  • Iso octane
  • Isopropyl alcohol
  • Lactic Acid Aq. (10%)
  • Lactic Acid Aq. (90%)
  • Lubricating Oils (Petroleum)
  • Magnesium Chloride Aq. (10%)
  • Magnesium Hydroxide Aq. (10%)
  • Magnesium Sulfide Aq. (10%)
  • Manganese Sulfate Aq. (10%)
  • Mercury
  • Methanol
  • Methyl Acetate
  • Methyl Ethyl Ketone
  • Methylene Chloride
  • Milk
  • Mineral Oils
  • Naphthalene
  • Nickel Sulfate Aq. (10%)
  • Nitric Acid Aq. (0.1%)
  • Nitric Acid Aq. (10%)
  • Nitrobenzene
  • Nitromethane
  • Oleic Acid
  • Oxalic Acid Aq. (10%)
  • Ozone
  • Paraffin
  • Perchloric Acid Aq. (10%)
  • Perchloroethylene
  • Petroleum Ether
  • Phenol Aq. (6%)
  • Phenol Aq. (75%)
  • Phosphoric Acid Aq (0.3%)
  • Phosphoric Acid Aq (3%)
  • Phosphoric Acid Aq. (10%)
  • Phthalic Acid Aq. (SAT)
  • Potassium Bicarbonate Aq. (60%)
  • Potassium Bromide Aq. (10%)
  • Potassium Carbonate Aq. (60%)
  • Potassium Chloride Aq. (90%)
  • Potassium Ferricyanide Aq. (30%)
  • Potassium Ferrocyanide Aq. (30%)
  • Potassium Hydroxide Aq. (10%)
  • Potassium Hydroxide Aq. (50%)
  • Potassium Permanganate Aq. (1%)
  • Potassium Sulfite Aq. (CONC)
  • Propane Gas
  • Resorcinol
  • Salicylic Acid
  • Silicone Fluids
  • Silver Nitrate
  • Soap Solutions
  • Sodium Acetate Aq. (60%)
  • Sodium Benzoate Aq. (10%)
  • Sodium Bicarbonate Aq. (50%)
  • Sodium Bisulphite Aq. (10%)
  • Sodium Bromide Aq. (10%)
  • Sodium Carbonate Aq. (20%)
  • Sodium Carbonate Aq. (50%)
  • Sodium Chlorate Aq. (10%)
  • Sodium Chloride Aq. (10%)
  • Sodium Chloride Aq. (90%)
  • Sodium Cyanide Aq. (10%)
  • Sodium Hydroxide Aq. (10%)
  • Sodium Hydroxide Aq. (50%)
  • Sodium Hypochlorite 15% CI (Chlorine Bleach)
  • Sodium Phosphates Aq. (General)
  • Sodium Sulfate Aq. (90%)
  • Sodium Sulfide Aq. (90%)
  • Sodium Thiosulfate Aq. (10%)
  • Stannic Chloride Aq. (10%)
  • Sulfur Dioxide (Dry Gas) (100%)
  • Sulfuric Acid Aq. (2%)
  • Sulfuric Acid Aq. (5%)
  • Sulfuric Acid Conc.
  • Sulfurous Acid Aq. (10%)
  • Tar
  • Tetrachlorethylene
  • Tetrahydrofuran
  • Toluene
  • Transformer Oil
  • Trichlorethylene
  • Triethanolamine
  • Trisodium Phosphate Aq. (95%)
  • Turpentine
  • Urea
  • Vaseline
  • Vegetable Oils
  • Vinegar
  • Vinyl Chloride
  • Water
  • Wax (Molten)
  • White Spirit
  • Wines & Spirits
  • Xylene
  • Zinc Chloride Aq. (10%)
  • Zinc Sulfate Aq. (10%)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。