Westlake Plastics HIPS High Impact Polystyrene

 

Subcategory: Polystyrene; Thermoplastic; Polymer

Material Notes:
HIPS is a low cost plastic material that is easy to machine and fabricate. It is often specified for low strength structural applications when impact resistance, machinability, and low cost are required. It is frequently used machining preproduction prototypes since it has excellent dimensional stability and is easy to fabricate. HIPS is FDA compliant for use in food processing applications.

Information provided by Westlake Plastics.

Available Properties
  • Cost, 1 to 10 (Nylon = 2)
  • Density
  • Hardness, Rockwell R
  • Tensile Strength @ Break
  • Tensile Strength @ Yield
  • Elongation at Break
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Yield Strength
  • Dimensional Stability (1-4; 4 = highest)
  • Izod Impact, Notched
  • CTE, linear 68°F
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Flammability, UL94
  • Clear
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。