Westlake Plastics Norylux™ 30% GF Modified Polyphenylene Oxide 30% glass filled
Subcategory: Polyphenylene Ether/PPO; Thermoplastic; Polymer;
Material Notes: Norylux modified PPO is a strong, engineering plastic with outstanding mechanical, thermal, and electric properties. Low moisture absorption and low thermal expansion make Norylux one of the most dimensionally stable thermoplastics available. It is used for a variety of structural applications including electrical housings, scientific instrumentation parts, and fluid handling components. Information provided by Westlake Plastics.
|
|
|
| Property Data |