Westlake Plastics Zelux® 40% GF Polycarbonate 40% Glass Filled
Subcategory: Polycarbonate; Thermoplastic; Polymer; ; ;
Material Notes: Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and impact strength are essential including lenses, manifolds, site glasses and machine guards. Zelux is used for a wide range of electrical applications since it has low moisture absorption and good insulating properties. Information provided by Westlake Plastics.
| Available Properties |
- Cost, 1 to 10 (Nylon = 2)
- Density
- Water Absorption
- Water Absorption at Saturation
- Hardness, Rockwell M
- Tensile Strength @ Yield
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Strength
- Compressive Modulus
- Machinability (1-10; 1 = easiest)
- Dimensional Stability (1-4; 4 = highest)
- Izod Impact, Unnotched
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 68°F
- Thermal Conductivity
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Black
- USP Class VI available
- Acetaldehyde Aq. (40%)
- Acetamide Aq. (50%)
- Acetic Acid Aq. (10%)
- Acetone
- Acrylonitrile
- Alcohols, Aliphatic
- Allyl Alcohol
- Aluminum Chloride Aq. (10%)
- Aluminum Sulfate Aq. (10%)
- Ammonia Aq. (10%)
- Ammonia Gas
- Ammonium Carbonate Aq. (10%)
- Ammonium Chloride Aq. (10%)
- Ammonium Chloride Aq. (37%)
- Amyl Acetate
- Amyl Alcohol
- Aniline
- Antimony Trichloride Aq. (10%)
- Barium Chloride Aq. (10%)
- Barium Sulfate Aq. (10%)
- Benzaldehyde
- Benzene
- Benzenesulfonic Acid
- Benzoic Acid Aq. (SAT)
- Benzyl Alcohol
- Beverages Aq. Alcoholic
- Beverages Aq. Carbonated
- Bitumen
- Boric Acid Aq. (10%)
- Bromine Aq. (30%)
- Bromine Liq.
- Butanol
- Butyl Acetate
- Butyl Phthalate
- Butylamine
- Butylene Glycol
- Butyric Acid (CONC)
- Butyric Acid Aq. (20%)
- Butyrolactone
- Calcium Chloride Aq. (10%)
- Calcium Hypochlorite
- Carbon Disulphide
- Carbon Tetrachloride
- Carbonic Acid Aq. (10%)
- Castor Oil
- Chlorine Aq. (10%)
- Chlorine Gas (100%)
- Chloroacetic Acid Aq. (10%)
- Chlorobenzene
- Chloroform
- Chlorosulfonic Acid Aq. (10%)
- Chrome Alum Aq. (10%)
- Chromic Acid Aq. (1%)
- Citric Acid Aq. (10%)
- Citric Acid Aq. (SAT)
- Creosote
- Cresols
- Cresylic Acid
- Cupric Chloride Aq. (10%)
- Cupric Sulfate Aq. (0.5%)
- Cupric Sulfate Aq. (10%)
- Cupric Sulfate Aq. (SAT)
- Cyclohexane
- Cyclohexanol
- Cyclohexanone
- Decalin
- Detergents, Organic
- Dibutylphthalate
- Dichlorodifluoro Methane
- Dichloroethylene
- Diesel Oil
- Diethyleneglycol Aq. (90%)
- Dimethyl Aniline
- Dimethyl Formamide
- Dioxane
- Edible Oils
- Ethanol, Denatured (96%)
- Ether, Diethyl
- Ethyl Acetate
- Ethyl Butyrate
- Ethyl Chloride
- Ethylene Chloride
- Ethylene Chlorohydrin
- Ethylene Diamine
- Ethylene Dichloride
- Ethylene Glycol Aq. (96%)
- Ferric Chloride Aq. (10%)
- Ferric Chloride Aq. (5%)
- Ferric Chloride Aq. (SAT)
- Ferrous Chloride Aq. (10%)
- Fluorine (Gas Wet)
- Fluorosilicic Acid Aq.
- Formaldehyde Aq. (10%)
- Formic Acid Aq. (10%)
- Formic Acid Aq. (3%)
- Freon 12 (Arcton 12)
- Fruit Juices (CONC)
- Furfural
- Gasoline
- Glycerine
- Heptane
- Hexane
- Hydrobromic Acid Aq. (10%)
- Hydrochloric Acid Aq. (0.4%)
- Hydrochloric Acid Aq. (10%)
- Hydrochloric Acid Aq. (2%)
- Hydrofluoric Acid Aq. (4%)
- Hydrogen Peroxide Aq. (0.5%)
- Hydrogen Peroxide Aq. (1%)
- Hydrogen Peroxide Aq. (3%)
- Hydrogen Sulfide Aq. (SAT)
- Hydrogenated Vegetable Oils
- Iodine (3%)
- Iodine (in Alcohol)
- Iso octane
- Isopropyl alcohol
- Isopropyl Ether
- Lactic Acid Aq. (10%)
- Lactic Acid Aq. (90%)
- Linseed Oil
- Lubricating Oils (Petroleum)
- Magnesium Chloride Aq. (10%)
- Magnesium Hydroxide Aq. (10%)
- Magnesium Sulfide Aq. (10%)
- Maleic Acid Aq. (CONC)
- Manganese Sulfate Aq. (10%)
- Mercuric Chloride Aq. (6%)
- Mercury
- Methanol
- Methyl Acetate
- Methyl Ethyl Ketone
- Methylene Chloride
- Milk
- Mineral Oils
- Nickel Sulfate Aq. (10%)
- Nitric Acid Aq. (0.1%)
- Nitric Acid Aq. (10%)
- Nitrobenzene
- Nitromethane
- Oleic Acid
- Oxalic Acid Aq. (10%)
- Ozone
- Paraffin
- Perchloric Acid Aq. (10%)
- Perchloroethylene
- Petroleum Ether
- Phenol (Molten)
- Phenol Aq. (6%)
- Phenol Aq. (75%)
- Phosphoric Acid Aq (0.3%)
- Phosphoric Acid Aq (3%)
- Phosphoric Acid Aq. (10%)
- Potassium Bromide Aq. (10%)
- Potassium Carbonate Aq. (60%)
- Potassium Chloride Aq. (90%)
- Potassium Dichromate Aq. (5%)
- Potassium Hydroxide Aq. (10%)
- Potassium Hydroxide Aq. (50%)
- Potassium Nitrate Aq. (10%)
- Potassium Permanganate Aq. (1%)
- Potassium Sulfite Aq. (CONC)
- Propane Gas
- Pyridine
- Resorcinol
- Salicylic Acid
- Silicone Fluids
- Silver Nitrate
- Soap Solutions
- Sodium Acetate Aq. (60%)
- Sodium Benzoate Aq. (10%)
- Sodium Bicarbonate Aq. (50%)
- Sodium Bisulphite Aq. (10%)
- Sodium Carbonate Aq. (20%)
- Sodium Carbonate Aq. (50%)
- Sodium Chlorate Aq. (10%)
- Sodium Chloride Aq. (10%)
- Sodium Chloride Aq. (90%)
- Sodium Cyanide Aq. (10%)
- Sodium Hydroxide Aq. (10%)
- Sodium Hydroxide Aq. (50%)
- Sodium Hypochlorite 15% CI (Chlorine Bleach)
- Sodium Nitrate Aq. (50%)
- Sodium Phosphates Aq. (General)
- Sodium Silicate
- Sodium Sulfate Aq. (90%)
- Sodium Sulfide Aq. (90%)
- Sodium Thiosulfate Aq. (10%)
- Stannic Chloride Aq. (10%)
- Stearic Acid
- Styrene (Monomer)
- Sulfur
- Sulfur Dioxide (Dry Gas) (100%)
- Sulfuric Acid Aq. (2%)
- Sulfuric Acid Aq. (5%)
- Sulfuric Acid Conc.
- Sulfurous Acid Aq. (10%)
- Tallow
- Tar
- Tartaric Acid Aq.
- Tetrachlorethylene
- Tetrahydrofuran
- Thionyl Chloride
- Thiophene
- Toluene
- Transformer Oil
- Trichlorethylene
- Triethanolamine
- Trisodium Phosphate Aq. (95%)
- Turpentine
- Urea
- Vaseline
- Vegetable Oils
- Vinegar
- Vinyl Chloride
- Water
- Wax (Molten)
- White Spirit
- Wines & Spirits
- Xylene
- Xylenol
- Zinc Chloride Aq. (10%)
- Zinc Sulfate Aq. (10%)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|