Material Notes: Carbon powder filled with high flexural strength and good thermal stability to 270°F. Thermoformable in 0.010" to 0.060" gauges; low outgassing.
Information provided by Westlake Plastics.
Available Properties
Density
Water Absorption
Hardness, Shore D
Tensile Strength @ Yield
Elongation at Break
Flexural Modulus
Flexural Strength
Machinability (1-10; 1 = easiest)
Dimensional Stability (1-4; 4 = highest)
Izod Impact, Unnotched
Izod Impact, Notched
Volume Resistivity
Surface Resistance
Static Decay
CTE, linear 68°F
Thermal Conductivity
Deflection Temperature at 1.8 MPa (264 psi)
Flammability, UL94
Black
USP Class VI available
Acetaldehyde Aq. (40%)
Acetamide Aq. (50%)
Acetic Acid Aq. (10%)
Acetone
Acrylonitrile
Alcohols, Aliphatic
Allyl Alcohol
Aluminum Chloride Aq. (10%)
Aluminum Sulfate Aq. (10%)
Ammonia Aq. (10%)
Ammonia Gas
Ammonium Carbonate Aq. (10%)
Ammonium Chloride Aq. (10%)
Ammonium Chloride Aq. (37%)
Amyl Acetate
Amyl Alcohol
Aniline
Antimony Trichloride Aq. (10%)
Barium Chloride Aq. (10%)
Barium Sulfate Aq. (10%)
Benzaldehyde
Benzene
Benzenesulfonic Acid
Benzoic Acid Aq. (SAT)
Benzyl Alcohol
Beverages Aq. Alcoholic
Beverages Aq. Carbonated
Bitumen
Boric Acid Aq. (10%)
Bromine Aq. (30%)
Bromine Liq.
Butanol
Butyl Acetate
Butyl Phthalate
Butylamine
Butylene Glycol
Butyric Acid (CONC)
Butyric Acid Aq. (20%)
Butyrolactone
Calcium Chloride Aq. (10%)
Calcium Hypochlorite
Carbon Disulphide
Carbon Tetrachloride
Carbonic Acid Aq. (10%)
Castor Oil
Chlorine Aq. (10%)
Chlorine Gas (100%)
Chloroacetic Acid Aq. (10%)
Chlorobenzene
Chloroform
Chlorosulfonic Acid Aq. (10%)
Chrome Alum Aq. (10%)
Chromic Acid Aq. (1%)
Citric Acid Aq. (10%)
Citric Acid Aq. (SAT)
Creosote
Cresols
Cresylic Acid
Cupric Chloride Aq. (10%)
Cupric Sulfate Aq. (0.5%)
Cupric Sulfate Aq. (10%)
Cupric Sulfate Aq. (SAT)
Cyclohexane
Cyclohexanol
Cyclohexanone
Decalin
Detergents, Organic
Dibutylphthalate
Dichlorodifluoro Methane
Dichloroethylene
Diesel Oil
Diethyleneglycol Aq. (90%)
Dimethyl Aniline
Dimethyl Formamide
Dioxane
Edible Oils
Ethanol, Denatured (96%)
Ether, Diethyl
Ethyl Acetate
Ethyl Butyrate
Ethyl Chloride
Ethylene Chloride
Ethylene Chlorohydrin
Ethylene Diamine
Ethylene Dichloride
Ethylene Glycol Aq. (96%)
Ferric Chloride Aq. (10%)
Ferric Chloride Aq. (5%)
Ferric Chloride Aq. (SAT)
Ferrous Chloride Aq. (10%)
Fluorine (Gas Wet)
Fluorosilicic Acid Aq.
Formaldehyde Aq. (10%)
Formic Acid Aq. (10%)
Formic Acid Aq. (3%)
Freon 12 (Arcton 12)
Fruit Juices (CONC)
Furfural
Gasoline
Glycerine
Heptane
Hexane
Hydrobromic Acid Aq. (10%)
Hydrochloric Acid Aq. (0.4%)
Hydrochloric Acid Aq. (10%)
Hydrochloric Acid Aq. (2%)
Hydrofluoric Acid Aq. (4%)
Hydrogen Peroxide Aq. (0.5%)
Hydrogen Peroxide Aq. (1%)
Hydrogen Peroxide Aq. (3%)
Hydrogen Sulfide Aq. (SAT)
Hydrogenated Vegetable Oils
Iodine (3%)
Iodine (in Alcohol)
Iso octane
Isopropyl alcohol
Isopropyl Ether
Lactic Acid Aq. (10%)
Lactic Acid Aq. (90%)
Linseed Oil
Lubricating Oils (Petroleum)
Magnesium Chloride Aq. (10%)
Magnesium Hydroxide Aq. (10%)
Magnesium Sulfide Aq. (10%)
Maleic Acid Aq. (CONC)
Manganese Sulfate Aq. (10%)
Mercuric Chloride Aq. (6%)
Mercury
Methanol
Methyl Acetate
Methyl Ethyl Ketone
Methylene Chloride
Milk
Mineral Oils
Nickel Sulfate Aq. (10%)
Nitric Acid Aq. (0.1%)
Nitric Acid Aq. (10%)
Nitrobenzene
Nitromethane
Oleic Acid
Oxalic Acid Aq. (10%)
Ozone
Paraffin
Perchloric Acid Aq. (10%)
Perchloroethylene
Petroleum Ether
Phenol (Molten)
Phenol Aq. (6%)
Phenol Aq. (75%)
Phosphoric Acid Aq (0.3%)
Phosphoric Acid Aq (3%)
Phosphoric Acid Aq. (10%)
Potassium Bromide Aq. (10%)
Potassium Carbonate Aq. (60%)
Potassium Chloride Aq. (90%)
Potassium Dichromate Aq. (5%)
Potassium Hydroxide Aq. (10%)
Potassium Hydroxide Aq. (50%)
Potassium Nitrate Aq. (10%)
Potassium Permanganate Aq. (1%)
Potassium Sulfite Aq. (CONC)
Propane Gas
Pyridine
Resorcinol
Salicylic Acid
Silicone Fluids
Silver Nitrate
Soap Solutions
Sodium Acetate Aq. (60%)
Sodium Benzoate Aq. (10%)
Sodium Bicarbonate Aq. (50%)
Sodium Bisulphite Aq. (10%)
Sodium Carbonate Aq. (20%)
Sodium Carbonate Aq. (50%)
Sodium Chlorate Aq. (10%)
Sodium Chloride Aq. (10%)
Sodium Chloride Aq. (90%)
Sodium Cyanide Aq. (10%)
Sodium Hydroxide Aq. (10%)
Sodium Hydroxide Aq. (50%)
Sodium Hypochlorite 15% CI (Chlorine Bleach)
Sodium Nitrate Aq. (50%)
Sodium Phosphates Aq. (General)
Sodium Silicate
Sodium Sulfate Aq. (90%)
Sodium Sulfide Aq. (90%)
Sodium Thiosulfate Aq. (10%)
Stannic Chloride Aq. (10%)
Stearic Acid
Styrene (Monomer)
Sulfur
Sulfur Dioxide (Dry Gas) (100%)
Sulfuric Acid Aq. (2%)
Sulfuric Acid Aq. (5%)
Sulfuric Acid Conc.
Sulfurous Acid Aq. (10%)
Tallow
Tar
Tartaric Acid Aq.
Tetrachlorethylene
Tetrahydrofuran
Thionyl Chloride
Thiophene
Toluene
Transformer Oil
Trichlorethylene
Triethanolamine
Trisodium Phosphate Aq. (95%)
Turpentine
Urea
Vaseline
Vegetable Oils
Vinegar
Vinyl Chloride
Water
Wax (Molten)
White Spirit
Wines & Spirits
Xylene
Xylenol
Zinc Chloride Aq. (10%)
Zinc Sulfate Aq. (10%)
Property Data
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below.