Westlake Plastics Propylux® CN-F Polypropylene (conductive)
Subcategory: Polypropylene; Thermoplastic; Polymer;
Material Notes: Non-sloughing, carbon-fiber-filled material with good chemical resistance, and high strength and stiffness and good temperature resistance to 215F. This material is light weight, easily machined and fabricated, and has good overall mechanical properties. Information provided by Westlake Plastics.
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|