Westlake Plastics Tempalux® CN-F Polyetherimide (conductive)
Subcategory: Polyetherimide; Thermoplastic; Polymer; ; ; ; ; ; ;
Material Notes: Non-sloughing carbon-fiber filled material which is extremely strong and stiff, has excellent dimensional stability, and high temperature resistance to 415F. This material has broad chemical resistance and excellent fabrication finishing characteristics. UL94 V-0 rated. Information provided by Westlake Plastics.
|
|
|