Westlake Plastics Absylux® CN-P Acrylonitrile-Butadiene-Styrene (conductive)
Subcategory: ABS Polymer; Thermoplastic; Polymer; ; ;
Material Notes: Carbon-powder-filled conductive material with high strength and stiffness, and relatively high impact strength. This material is easily machined and fabricated into close tolerance finished parts. Information provided by Westlake Plastics.
|
|
|