Westlake Plastics PVDF CN-P KYNAR® Polyvinylidene Fluoride (conductive)
Subcategory: Fluoropolymer; Thermoplastic; PVDF; Polymer; ; ; ; ;
Material Notes: Carbon-powder-filled, thermally stable, conductive material with consistent resistivities <10^5. This material is extremely tough with good flame and abrasion resistance. Resistant to many chemistries and solvents, including strong acids. Due to the carbon powder fill, this material is also available in film format as thin as .002". Kynar® is a trade name of Elf Atochem North America. Information provided by Westlake Plastics.
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|