Westlake Plastics PEEK® Film Made from VICTREX® Polymer
Subcategory: Polyketone; Polyetheretherketone (PEEK); Thermoplastic; Polymer; ; ; ; ; ; ;
Material Notes: Extremely high temperature resistance and continuous use temperature. Excellent flexural and tensile properties. Good abrasion and rain erosion resistance. Excellent chemical resistance. Excellent electrical properties. Information provided by Westlake Plastics.
|
|
|