Westlake Plastics PMP Film Made from TPX® Polymethylpentene Resin
Subcategory: Polymethylpentene; Thermoplastic; Polymer
Material Notes: Lowest specific gravity of any known thermoplastic. Exceptional electrical properties. Good chemical resistance. High heat resistance. Excellent acoustical properties. Transparency. FDA compliant. TPX® is a trade name of Mitsui Plastics Inc. Information provided by Westlake Plastics.
| Available Properties |
- Cost, 1 to 10 (Nylon = 2)
- Density
- Water Absorption
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Dimensional Stability (1-4; 4 = highest)
- Tear Strength
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Flammability, UL94
- Oxygen Index
- Refractive Index
- Haze
- Natural (off white)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|