Westlake Plastics Radel® R 4400 Polyphenylsulfone For Medical Applications
Subcategory: Polyphenylsulfone; Thermoplastic; Polymer; ; ; ; ; ;
Material Notes: Medical grade Radel R4400 resin offers exceptional hydrolytic stability, toughness, heat deflection temperature and resistance to stress cracking. This polymer also has excellent thermal stability, and impact strength over a wide temperature range. Recommended sterilization techniques for Radel R4400 include EtO gas, radiation, steam autoclaving, dry heat and cold sterilization. Radel® is a trade name of Solvay Advanced Polymers. Information provided by Westlake Plastics.
| Available Properties |
- Cost, 1 to 10 (Nylon = 2)
- Density
- Water Absorption
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Compressive Modulus
- Dimensional Stability (1-4; 4 = highest)
- Izod Impact, Unnotched
- Tensile Impact Strength
- Izod Impact, Notched
- CTE, linear 68°F
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Black
- White
- Amber
- Green
- Blue
- Brown
- Grey
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|