Westlake Plastics Tempalux® Polyetherimide

 

Subcategory: Polyetherimide; Thermoplastic; Polymer; ; ; ; ; ; ;

Material Notes:
An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad chemical resistance. Tempalux stock shapes are inherently flame resistant with low smoke emission. Tempalux stock shapes display property retention and resistance to environmental stress cracking when exposed to a wide variety of chemicals. The standard color of Tempalux stock shapes is light amber. Glass filled grades appear tan or greenish in color.

Information provided by Westlake Plastics.

Available Properties
  • Cost, 1 to 10 (Nylon = 2)
  • Density
  • Water Absorption
  • Hardness, Rockwell M
  • Tensile Strength @ Yield
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Yield Strength
  • Compressive Yield Strength
  • Compressive Modulus
  • Machinability (1-10; 1 = easiest)
  • Dimensional Stability (1-4; 4 = highest)
  • Izod Impact, Unnotched
  • Izod Impact, Notched
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 68°F
  • Thermal Conductivity
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Flammability, UL94
  • Oxygen Index
  • Black
  • Amber
  • Transparent
  • FDA
  • USDA
  • NSF
  • USP Class VI available
  • Autoclavable
  • UV Resistance (1-4; 4 = highest)
  • Outgassing (% TML) (1-4; 4 = highest)
  • Acetaldehyde Aq. (40%)
  • Acetic Acid Aq. (10%)
  • Acetone
  • Alcohols, Aliphatic
  • Ammonia Aq. (10%)
  • Amyl Acetate
  • Benzaldehyde
  • Benzene
  • Benzoic Acid Aq. (SAT)
  • Beverages Aq. Alcoholic
  • Beverages Aq. Carbonated
  • Butanol
  • Butyl Acetate
  • Butylamine
  • Butylene Glycol
  • Carbon Tetrachloride
  • Chloroform
  • Chromic Acid Aq. (1%)
  • Citric Acid Aq. (10%)
  • Citric Acid Aq. (SAT)
  • Cyclohexane
  • Cyclohexanol
  • Decalin
  • Detergents, Organic
  • Dibutylphthalate
  • Dichlorodifluoro Methane
  • Dichloroethylene
  • Diesel Oil
  • Dimethyl Formamide
  • Edible Oils
  • Ethanol, Denatured (96%)
  • Ether, Diethyl
  • Ethyl Acetate
  • Ethyl Butyrate
  • Ethylene Chloride
  • Ethylene Diamine
  • Ethylene Dichloride
  • Ethylene Glycol Aq. (96%)
  • Ferrous Chloride Aq. (10%)
  • Formaldehyde Aq. (10%)
  • Formic Acid Aq. (10%)
  • Formic Acid Aq. (3%)
  • Freon 12 (Arcton 12)
  • Gasoline
  • Glycerine
  • Heptane
  • Hexane
  • Hydrochloric Acid Aq. (0.4%)
  • Hydrochloric Acid Aq. (10%)
  • Hydrochloric Acid Aq. (2%)
  • Hydrofluoric Acid Aq. (4%)
  • Hydrogen Peroxide Aq. (0.5%)
  • Hydrogen Peroxide Aq. (1%)
  • Hydrogen Peroxide Aq. (3%)
  • Hydrogen Sulfide Aq. (SAT)
  • Iodine (3%)
  • Iso octane
  • Isopropyl alcohol
  • Isopropyl Ether
  • Lubricating Oils (Petroleum)
  • Methanol
  • Methyl Acetate
  • Methyl Ethyl Ketone
  • Methylene Chloride
  • Milk
  • Mineral Oils
  • Naphthalene
  • Nitric Acid Aq. (0.1%)
  • Nitric Acid Aq. (10%)
  • Nitrobenzene
  • Oxalic Acid Aq. (10%)
  • Ozone
  • Paraffin
  • Perchloroethylene
  • Petroleum Ether
  • Phenol (Molten)
  • Phenol Aq. (6%)
  • Phenol Aq. (75%)
  • Phosphoric Acid Aq (0.3%)
  • Phosphoric Acid Aq (3%)
  • Phosphoric Acid Aq. (10%)
  • Potassium Carbonate Aq. (60%)
  • Potassium Hydroxide Aq. (10%)
  • Potassium Hydroxide Aq. (50%)
  • Propane Gas
  • Silicone Fluids
  • Soap Solutions
  • Sodium Acetate Aq. (60%)
  • Sodium Benzoate Aq. (10%)
  • Sodium Bicarbonate Aq. (50%)
  • Sodium Bisulphite Aq. (10%)
  • Sodium Carbonate Aq. (20%)
  • Sodium Carbonate Aq. (50%)
  • Sodium Chlorate Aq. (10%)
  • Sodium Chloride Aq. (10%)
  • Sodium Chloride Aq. (90%)
  • Sodium Cyanide Aq. (10%)
  • Sodium Hydroxide Aq. (10%)
  • Sodium Hydroxide Aq. (50%)
  • Sodium Hypochlorite 15% CI (Chlorine Bleach)
  • Sodium Nitrate Aq. (50%)
  • Sodium Perborate Aq. (10%)
  • Sodium Phosphates Aq. (General)
  • Sodium Silicate
  • Sodium Sulfate Aq. (90%)
  • Sodium Sulfide Aq. (90%)
  • Sodium Thiosulfate Aq. (10%)
  • Stannic Chloride Aq. (10%)
  • Sulfuric Acid Aq. (2%)
  • Sulfuric Acid Aq. (5%)
  • Sulfuric Acid Conc.
  • Sulfurous Acid Aq. (10%)
  • Tallow
  • Tetrachlorethylene
  • Tetrahydrofuran
  • Toluene
  • Trichlorethylene
  • Triethanolamine
  • Trisodium Phosphate Aq. (95%)
  • Vaseline
  • Vegetable Oils
  • Vinegar
  • Vinyl Chloride
  • Water
  • Wax (Molten)
  • Wines & Spirits
  • Xylene
  • Xylenol
  • Zinc Chloride Aq. (10%)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。