Westlake Plastics Halar® 901 ECTFE
Subcategory: Fluoropolymer; Thermoplastic; ETFE/ECTFE; Polymer
Material Notes: Made from HALAR® ethylene-cholorotrifluoroethylene resin, these products are virtually unaffected by most corrosive chemicals. ECTFE products have excellent chemical and mechanical properties, impact strength, and a broad service use temperature. This polymer offers extremely low permeability to liquids, gases, and vapors. Halar® is a trade name of Solvay Solexis, Inc. Information provided by Westlake Plastics.
|
|
|