Westlake Plastics Kynar® 740/1000HD PVDF Homopolymer, Compression Molded
Subcategory: Fluoropolymer; Thermoplastic; PVDF; Polymer; ; ; ;
Material Notes: Compression molded, manufactured from Kynar polyvinylidene fluoride resin. This material offers excellent corrosion and chemical resistance at both ambient and elevated temperatures. PVDF is also inherently UV stable, mechanically tough, abrasion and flame resistant. Kynar 1000HD is a whiter grade of PVDF than Kynar 740. Kynar® is a trade name of Elf Atochem North America. Information provided by Westlake Plastics.
| Available Properties |
- Cost, 1 to 10 (Nylon = 2)
- Density
- Water Absorption
- Hardness, Shore D
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Machinability (1-10; 1 = easiest)
- Dimensional Stability (1-4; 4 = highest)
- Izod Impact, Unnotched
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- CTE, linear 68°F
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Natural (off white)
- FDA
- USDA
- 3A-Dairy
- Autoclavable
- Acetaldehyde Aq. (40%)
- Acetamide Aq. (50%)
- Acetic Acid Aq. (10%)
- Acetone
- Acrylonitrile
- Alcohols, Aliphatic
- Allyl Alcohol
- Allyl Chloride
- Aluminum Chloride Aq. (10%)
- Aluminum Sulfate Aq. (10%)
- Ammonia Aq. (10%)
- Ammonia Gas
- Ammonium Carbonate Aq. (10%)
- Ammonium Chloride Aq. (10%)
- Ammonium Chloride Aq. (37%)
- Amyl Acetate
- Amyl Alcohol
- Aniline
- Antimony Trichloride Aq. (10%)
- Barium Chloride Aq. (10%)
- Barium Sulfate Aq. (10%)
- Barium Sulfide Aq. (10%)
- Benzaldehyde
- Benzene
- Benzenesulfonic Acid
- Benzoic Acid Aq. (SAT)
- Benzyl Alcohol
- Bitumen
- Bleaching Lye (10%)
- Boric Acid Aq. (10%)
- Boron Trifluoride
- Bromine Aq. (30%)
- Bromine Liq.
- Butanol
- Butyl Acetate
- Butyl Phthalate
- Butylene Glycol
- Butyric Acid (CONC)
- Butyric Acid Aq. (20%)
- Calcium Chloride Aq. (10%)
- Calcium Hypochlorite
- Carbon Disulphide
- Carbon Tetrachloride
- Carbonic Acid Aq. (10%)
- Castor Oil
- Chloral Hydrate
- Chlorine Aq. (10%)
- Chlorine Gas (100%)
- Chloroacetic Acid Aq. (10%)
- Chlorobenzene
- Chloroform
- Chlorosulfonic Acid Aq. (10%)
- Chromic Acid Aq. (1%)
- Citric Acid Aq. (10%)
- Citric Acid Aq. (SAT)
- Coconut Oil
- Creosote
- Cresols
- Cresylic Acid
- Cupric Chloride Aq. (10%)
- Cupric Sulfate Aq. (0.5%)
- Cupric Sulfate Aq. (10%)
- Cupric Sulfate Aq. (SAT)
- Cyclohexane
- Cyclohexanol
- Cyclohexanone
- Detergents, Organic
- Dibutylphthalate
- Dichlorodifluoro Methane
- Dichloroethylene
- Diesel Oil
- Diethyleneglycol Aq. (90%)
- Dimethyl Aniline
- Dimethyl Formamide
- Dioxane
- Edible Oils
- Ethanol, Denatured (96%)
- Ether, Diethyl
- Ethyl Acetate
- Ethyl Butyrate
- Ethyl Chloride
- Ethylene Chloride
- Ethylene Chlorohydrin
- Ethylene Diamine
- Ethylene Dichloride
- Ethylene Glycol Aq. (96%)
- Ferric Chloride Aq. (10%)
- Ferric Chloride Aq. (5%)
- Ferric Chloride Aq. (SAT)
- Ferrous Chloride Aq. (10%)
- Fluorine (Gas Wet)
- Fluorosilicic Acid Aq.
- Formaldehyde Aq. (10%)
- Formic Acid Aq. (10%)
- Formic Acid Aq. (3%)
- Freon 12 (Arcton 12)
- Fruit Juices (CONC)
- Furfural
- Gasoline
- Glycerine
- Heptane
- Hexane
- Hydrobromic Acid Aq. (10%)
- Hydrochloric Acid Aq. (0.4%)
- Hydrochloric Acid Aq. (10%)
- Hydrochloric Acid Aq. (2%)
- Hydrofluoric Acid Aq. (4%)
- Hydrogen Peroxide Aq. (0.5%)
- Hydrogen Peroxide Aq. (1%)
- Hydrogen Peroxide Aq. (3%)
- Hydrogen Sulfide Aq. (SAT)
- Hydrogenated Vegetable Oils
- Hydroquinone
- Iodine (3%)
- Iodine (in Alcohol)
- Iso octane
- Isopropyl alcohol
- Isopropyl Ether
- Lactic Acid Aq. (10%)
- Lactic Acid Aq. (90%)
- Lead Acetate Aq. (10%)
- Linseed Oil
- Lithium Bromide Aq. (50%)
- Lubricating Oils (Petroleum)
- Magnesium Chloride Aq. (10%)
- Magnesium Hydroxide Aq. (10%)
- Maleic Acid Aq. (CONC)
- Manganese Sulfate Aq. (10%)
- Mercuric Chloride Aq. (6%)
- Mercury
- Methanol
- Methyl Acetate
- Methyl Ethyl Ketone
- Methylene Chloride
- Methylpyrrolidone
- Milk
- Mineral Oils
- Naphthalene
- Nickel Sulfate Aq. (10%)
- Nicotine
- Nitric Acid Aq. (0.1%)
- Nitric Acid Aq. (10%)
- Nitrobenzene
- Nitromethane
- Oleic Acid
- Oxalic Acid Aq. (10%)
- Ozone
- Paraffin
- Perchloric Acid Aq. (10%)
- Perchloroethylene
- Petroleum Ether
- Phenol Aq. (6%)
- Phenol Aq. (75%)
- Phosphoric Acid Aq (0.3%)
- Phosphoric Acid Aq (3%)
- Phosphoric Acid Aq. (10%)
- Phthalic Acid Aq. (SAT)
- Potassium Acetate Aq. (50%)
- Potassium Bicarbonate Aq. (60%)
- Potassium Bromide Aq. (10%)
- Potassium Carbonate Aq. (60%)
- Potassium Chloride Aq. (90%)
- Potassium Dichromate Aq. (5%)
- Potassium Ferricyanide Aq. (30%)
- Potassium Ferrocyanide Aq. (30%)
- Potassium Hydroxide Aq. (10%)
- Potassium Hydroxide Aq. (50%)
- Potassium Permanganate Aq. (1%)
- Potassium Sulfite Aq. (90%)
- Potassium Sulfite Aq. (CONC)
- Propane Gas
- Pyridine
- Salicylic Acid
- Silicone Fluids
- Silver Nitrate
- Soap Solutions
- Sodium Acetate Aq. (60%)
- Sodium Benzoate Aq. (10%)
- Sodium Bicarbonate Aq. (50%)
- Sodium Bisulphite Aq. (10%)
- Sodium Bromide Aq. (10%)
- Sodium Carbonate Aq. (20%)
- Sodium Carbonate Aq. (50%)
- Sodium Chlorate Aq. (10%)
- Sodium Chloride Aq. (10%)
- Sodium Chloride Aq. (90%)
- Sodium Cyanide Aq. (10%)
- Sodium Hydroxide Aq. (10%)
- Sodium Hydroxide Aq. (50%)
- Sodium Hypochlorite 15% CI (Chlorine Bleach)
- Sodium Nitrate Aq. (50%)
- Sodium Perborate Aq. (10%)
- Sodium Phosphates Aq. (General)
- Sodium Silicate
- Sodium Sulfate Aq. (90%)
- Sodium Sulfide Aq. (90%)
- Sodium Thiosulfate Aq. (10%)
- Stannic Chloride Aq. (10%)
- Stearic Acid
- Styrene (Monomer)
- Sulfur
- Sulfur Dioxide (Dry Gas) (100%)
- Sulfuric Acid Aq. (2%)
- Sulfuric Acid Aq. (5%)
- Sulfuric Acid Conc.
- Sulfurous Acid Aq. (10%)
- Tallow
- Tar
- Tartaric Acid Aq.
- Tetrachlorethylene
- Tetrahydrofuran
- Thionyl Chloride
- Toluene
- Transformer Oil
- Trichlorethylene
- Triethanolamine
- Trisodium Phosphate Aq. (95%)
- Turpentine
- Urea
- Vaseline
- Vegetable Oils
- Vinegar
- Vinyl Chloride
- Water
- White Spirit
- Wines & Spirits
- Xylene
- Zinc Chloride Aq. (10%)
- Zinc Oxide
- Zinc Sulfate Aq. (10%)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|