Washington Penn PPC3MF1.5-Black Polypropylene, 15% Mica-Filled, Chemically-Coupled
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Heat Stabilized injection molding compound. Meets physical requirements for General Motors Spec. GMP.PP.024. Applications: HVAC duct and other various automotive applications. Data provided by Washington Penn Plastic Co., Inc.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|