Washington Penn PPH3TF4-BLK Polypropylene, 40% Talc Filled
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Homopolymer. Meets GMP.PP.030 spec. Applications: Fan shrouds, heater housings, various under hood uses. Data provided by Washington Penn Plastic Co., Inc.