Washington Penn PPH5CF75 Polypropylene, 75% Calcium Carbonate Filled Concentrate
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: UV Stabilized. Applications: Shelving Data provided by Washington Penn Plastic Co., Inc.
|
|
|