Zakłady Azotowe TARNOFORM 300 DW POM
Subcategory: Acetal; Thermoplastic
Material Notes: Tribological modified grade with combination of damping and wear reducing additives. Finished parts have low coefficient of friction and wear with reduction of acoustic emission during sliding. Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Ball Indentation Hardness
- Tensile Strength, Yield
- Elongation at Break
- Flexural Strength
- Charpy Impact, Notched
- Izod Impact, Notched (ISO)
- Volume Resistivity
- Surface Resistance
- Comparative Tracking Index
- Specific Heat Capacity
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Processing Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|