Zakłady Azotowe TARNAMID T-27 GF25 NYLON 6
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: 25% glass fibers, release agent and standard stabilization system to improve resistance of material against temperature influence. Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Ball Indentation Hardness
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Izod Impact, Notched (ISO)
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Comparative Tracking Index
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Glow Wire Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|