Zakłady Azotowe TARFLEN ST PTFE
Subcategory: Fluoropolymer; Thermoplastic; PTFE
Material Notes: Free-Flowing suspension powder for ram extrusion of rods, pipes and other profiles. Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
| Available Properties |
- Density
- Bulk Density
- Particle Size
- Hardness, Shore D
- Ball Indentation Hardness
- Tensile Strength, Yield
- Elongation at Break
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- Comparative Tracking Index
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Flammability, UL94
- Mold Temperature
- Back Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|