Alcar General Purpose Prime Acetal
Subcategory: Acetal; Thermoplastic
Close Analogs: No response from Alcar Services has been received for many years. MatWeb believes it is no longer in the plastics business.
Material Notes: Data provided by the supplier, Alcar Services, Inc, Albertson, NY.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell M
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Coefficient of Friction
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|