Zell-Metall Engineering Plastics ZELLAMID® 1200 G
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Zellamid® 1200 G is manufactured by an activated anionic reaction. Finished and semi-finished parts are produced by a static cast process. This process makes it possible to produce a material with high molecular weight, high crystallinity and very low inner stress level. Zellamid® 1200 G is showing significant low moisture absorption, superior dimensional stability combined with high impact strength even at low temperatures and an excellent chemical resistance.Zellamid® 1200 G is the ideal longterm solution for bushes, bearings, rollers and gear wheels subjected to high load and wear demanding for dimensional stability particularly when exposed to high humidity and water.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Hardness, Shore D
- Ball Indentation Hardness
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Coefficient of Friction
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flammability, UL94
- Permissible Unit Pressure
- Time yield limit
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|