Zeon Chemicals Zeotherm® 120-90B Thermoplastic Vulcanizate
Subcategory: Elastomer, TPE; Thermoplastic; Thermoplastic Vulcanizate Elastomer (TPV)
Material Notes: A high-performance thermoplastic vulcanizate (TPV) designed to survive long-term exposure to 150°C (300°F) air and oil. Specifically designed for automotive air ducts, boots and bellows including CVJ boots, prop shaft boots, and rack-and-pinion boots.
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Compression Set, Elevated Temperature
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Melt Temperature
- Elongation at break, change
- Hardness Change
- Tensile Strength Change
- Volume Change
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|