Zeon Chemicals Nipol® 1001LG Nitrile Elastomer

 

Subcategory: Elastomer, TS; Thermoset

Key Words: NBR

Material Notes:
Nipol 1001LG is a copolymer of butadiene and acrylonitrile with very high oil resistance. Its properties are similar to those of Nipol 1001CG with the exception that: a) nomilling is required for ungelled cements; and b) non-polymer constituents have been designed so as not to interfere with adhesion. Sufficient antioxidant is added during manufacture for normal storage conditions. No fatty acid or fatty soap is used in the manufacturing process for this product.

Similar to 1001CG, but can be dissolved in solvents without milling. Contains no fatty acids or soaps.

Available Properties
  • Specific Gravity
  • Viscosity
  • Mooney Viscosity
  • Ash
  • AO Type
  • Bound ACN (%, acrylonitrile)
  • Heat Loss (%) Max
  • Hot/Cold
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。