Zeon Chemicals Nipol® 1002 Nitrile Elastomer
Subcategory: Elastomer, TS; Thermoset
Key Words: NBR
Material Notes: Nipol 1002 is a copolymer of butadiene and acrylonitrile with medium oil resistance. Sufficient non-staining antioxidant is added during manufacture for normal storage conditions.The original medium-high ACN. Provides good long-term water resistance.