Zeon Chemicals Nipol® 33-5SR Nitrile Elastomer
Subcategory: Elastomer, TS; Thermoset
Key Words: NBR
Material Notes: Special-purpose, intermediate-viscosity nitrile rubber designed to provide maximum processing safety without fouling molds. Recommended for high-temperature injection molding of parts.Special purpose, intermediate-viscosity nitrile rubber designed to provide maximum processing safety without fouling molds. Recommended for high-temperature injection molding of parts.
| Available Properties |
- Specific Gravity
- Mooney Viscosity
- Ash
- AO Type
- Bound ACN (%, acrylonitrile)
- Heat Loss (%) Max
- Hot/Cold
|
|
|
|