Zeon Chemicals Nipol® 1094-80 Nitrile Elastomer
Subcategory: Elastomer, TS; Thermoset
Key Words: NBR
Material Notes: Nipol 1094-80 is a copolymer of butadiene and acrylonitrile with low oil resistance, developed for low temperature flexibility. Sufficient non-staining antioxidant is added during manufacture for normal storage conditions.Low-temperature resistance with outstanding physical properties.
| Available Properties |
- Specific Gravity
- Mooney Viscosity
- Ash
- Transformation Temperature, Tg
- AO Type
- Bound ACN (%, acrylonitrile)
- Heat Loss (%) Max
- Hot/Cold
|
|
|
|