Zeon Chemicals Nipol® NX775 Carboxylated Nitrile Elastomer
Subcategory: Elastomer, TS; Thermoset
Key Words: NBR
Material Notes: Nipol NX775 is a cold polymerized, butadiene-acrylonitrile-carboxylic acid terpolymer. Sufficient non-staining antioxidant is added during manufacture for normal storage conditions.Excellent processing with conventional coated zinc oxides. High performance injection molding, rolls, calendered belting and extruded hose. Fast cure rate. Carboxyl content is 0.083 EPHR.
| Available Properties |
- Specific Gravity
- Mooney Viscosity
- Ash
- AO Type
- Bound ACN (%, acrylonitrile)
- Carboxyl Content, %
- Heat Loss (%) Max
- Hot/Cold
- Mooney Scorch MS, Min
|
|
|
|