Zeon Chemicals Nipol® 1072CGX Carboxylated Nitrile Elastomer
Subcategory: Elastomer, TS; Thermoset
Key Words: NBR
Material Notes: Nipol 1072CGX is a copolymer of butadiene and acrylonitrile with medium oil resistance modified to contian free carboxylic groups and is soluble in MEK without mill brakdown. Sufficient antioxidant is added during manufacture for normal storage conditions.Cement grade version of Nipol 1072.
| Available Properties |
- Specific Gravity
- Viscosity
- Mooney Viscosity
- Ash
- AO Type
- Bound ACN (%, acrylonitrile)
- Carboxyl Content, %