Zeon Chemicals Nipol® 1312 Liquid Nitrile Elastomer
Subcategory: Elastomer, TS; Thermoset
Key Words: NBR
Material Notes: Nipol 1312 is a copolymer of butadiene and acrylonitrile with medium oil resistance in liquid form. Sufficient antioxidant is added during manufacture for normal storage conditions.Plasticizer used for nitrile, neoprene and PVC compounds. Improves knitting and flow. May also be used in plastisols and phenolic resins.
| Available Properties |
- Specific Gravity
- Brookfield Viscosity
- Ash
- AO Type
- Bound ACN (%, acrylonitrile)
- Heat Loss (%) Max
- Hot/Cold
|
|
|
|
| Property Data |