Zeon Chemicals Nipol® 9010 Polyblack Masterbatch
Subcategory: Elastomer, TS; Thermoset
Key Words: NBR
Material Notes: Nipol® nitrile elastomers are recommended when oil or solvent resistance is needed for the proper functioning of rubber parts. Fuel, oil and solvent resistance improves as acrylonitrile content is increased. Low temperature flexibility and resiliency are improved as butadiene content increases.Recommended for use in mechanical goods requiring medium-high solvent and oil resistance.
| Available Properties |
- Specific Gravity
- Mooney Viscosity
- Carbon Black Loading
- Ash
- AO Type
- Bound ACN (%, acrylonitrile)
- Heat Loss (%) Max
- Hot/Cold
- Nipol Base Polymer
|
|
|
|
| Property Data |