Zeon Chemicals Nipol® 1472HV Nitrile Powder and Crumb Elastomer
Subcategory: Elastomer, TS; Thermoset
Key Words: NBR
Material Notes: Nipol® nitrile elastomers are recommended when oil or solvent resistance is needed for the proper functioning of rubber parts. Fuel, oil and solvent resistance improves as acrylonitrile content is increased. Low temperature flexibility and resiliency are improved as butadiene content increases.Carboxylated nitrile crumb with talc partitioning agent.
| Available Properties |
- Particle Size
- Mooney Viscosity
- Transformation Temperature, Tg
- Hot/Cold
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal