Zeon Chemicals Sivic® Z740 Polyblend Nitrile Elastomer
Subcategory: Vinyl; Elastomer, TS; Thermoset
Key Words: NBR/PVC
Material Notes: Sivic Z740 is a fully fluxed polyblend of 41% ACB NBR/PVC (70/30). IT is produced via a mechanical technology, which provides a lump-free homogenous polymer.High ACN content for improved fuel resistance in automotive applications.
| Available Properties |
- Specific Gravity
- Mooney Viscosity
- Bound ACN (%, acrylonitrile)
- NBR/PVC Ratio
- Type
|
|
|
|
| Property Data |