Zeon Chemicals Sivic® Z702 Polyblend Nitrile Elastomer
Subcategory: Vinyl; Elastomer, TS; Thermoset
Key Words: NBR/PVC
Material Notes: Sivic Z702 is a fully fluxed polyblend of 23% ACN NBR/PVC (70/30). It is produced via a mechanical technology, which provides a lump-free homogenous polymer.Lowest ACN content for improved cold flexibility. Automotive and industrial cable, hose, and belt applications.