Zeon Chemicals Zetpol® 2000LL Hydrogenated Nitrile Elastomomers
Subcategory: Elastomer, TS; Thermoset
Key Words: HNBR
Material Notes: Zeptol 2000LL is the lowest Mooney version of a highly saturatred copolymer of butadiene and acrylonitrile with high tensile strength, excellent heat resistance, good chemcial resistance to aggressive fluids, and an excellent balance of properties over a wide variation of temperatures.Ultra-low Mooney version of Zetpol 2000. Excellent for transfer or injection molding. O-rings, seals, gaskets, blow-out preventers. FDA approved.
| Available Properties |
- Specific Gravity
- Iodine Absorption Number
- Mooney Viscosity
- Ash
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- 300% Modulus
- % HYD
- Bound ACN (%, acrylonitrile)
- Heat Loss (%) Max
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|