Zeon Chemicals Zetpol® 3310 Hydrogenated Nitrile Elastomomers
Subcategory: Elastomer, TS; Thermoset
Key Words: HNBR
Material Notes: Zetpol 3310 is a highly saturated terpolymer of butadiene, acrylonitrile, and a proprietary third monomer with good tensile strength, excellent heat resistance, excellent lowtemperature flexibility, and an excellent balance of properties over a wide variation of temperatures.Improved low-temperature performance (TR10 of -33°C) providing a good balance of oil and low-temperature resistance plus improved high temperature capabilities.
| Available Properties |
- Specific Gravity
- Iodine Absorption Number
- Mooney Viscosity
- Ash
- % HYD
- Bound ACN (%, acrylonitrile)
- Heat Loss (%) Max
|
|
|
|