Zeon Chemicals HyTemp® AR71 AR Polyacrylate Elastomers
Subcategory: Elastomer, TS; Acrylic; Thermoset
Key Words: ACM
Material Notes:
175°C high-temperature service and excellent oil resistance.
| Available Properties |
- Specific Gravity
- Minimum Service Temperature, Air
- % Volume Swell
- Curesite
|
|
|
|