Zeon Chemicals HyTemp® AR12 AR Super ACM Polyacrylate Elastomers
Subcategory: Elastomer, TS; Acrylic; Thermoset
Key Words: ACM
Material Notes:
Curesite is optimized for improved long-term heat and compression set resistance over traditional acrylates with good low-temperature properties.
| Available Properties |
- Specific Gravity
- Mooney Viscosity
- Minimum Service Temperature, Air
- % Volume Swell
- Curesite
|
|
|
|